Field Note

Telling a Weak Cell from a Bad Sense Wire

black and white solar panels
Photo by Nuno Marques on Unsplash

One cell sits twenty millivolts below the rest. It has done so for a week. The BMS reports it, the app shows it, and the obvious conclusion is that the cell is failing. It might be. It might also be a sense wire with a bad crimp, and replacing a cell because of a crimp is an expensive way to learn the difference.

The two causes produce nearly the same number, so the reading alone cannot separate them. What separates them is where the voltage is measured and how it behaves.

Measure at the terminal, not through the BMS

A BMS measures cell voltage through thin sense wires and a connector. A meter measures it at the metal. Put the meter probes directly on the cell terminals at the same moment the app shows the value, and compare. If the meter says 3.31 V and the app says 3.09 V, the cell is fine and something between the terminal and the BMS is losing 220 mV. If both say 3.09 V, the cell is genuinely low.

This single comparison settles most cases, and it costs nothing. It also tells you how much is being lost, which is useful on its own: a 200 mV drop in a sense path is a fault, not a tolerance.

Swap the lead

If the reading and the meter agree, the next check is still cheap. Power the pack down and move the suspect cell's sense lead to a neighbouring cell's connector position, one that you know reads correctly. Power up and look at the app:

  • The fault moves. The bad reading follows the wire, so the wire or its connector is the problem.
  • The fault stays. The same cell position reads low whatever wire feeds it, so the cell is the problem.

Do not do this live. Sense connectors are not rated for being moved under load, and a probe that slips across adjacent pins is a short across cells.

Read the resistance field

Many JK-BMS units report a per-cell wire resistance, usually in milliohms. It is not a precision measurement, but it is comparative: one cell with several times the resistance of its neighbours is a joint, a crimp or a fuse, not chemistry. A high resistance cell often reads low under load and recovers at rest, which brings us to the next test.

Watch it under load and at rest

Rest the pack for an hour and record the cell voltages. Then apply a steady load and record again. A weak cell sags further under load than its neighbours and recovers slowly when the load goes away. A resistive path behaves differently: the drop appears with current and disappears almost immediately when the current stops, because the loss is in the connection rather than in stored energy.

Self-discharge is the third pattern. Leave the pack disconnected for several days. A cell that falls away from the others with no load at all is losing charge internally. That is a cell problem, and no amount of balancing fixes it. The self-discharge test is worth doing before you replace anything.

What the numbers do not tell you

A monitoring app shows the pattern, not the cause. It can show you that cell 7 is consistently low, that it sags harder under load, and that it recovers slowly. It cannot see the crimp. The meter and the swap do that, and they are the two minutes that decide whether you buy a cell or a connector.

If you want the pattern recorded rather than watched, the JK BMS Bluetooth app keeps cell deltas and per-cell readings on the screen and in history, which makes a comparison over a week much easier than squinting at a live value. It is a measurement aid. It does not replace the BMS protection, and it does not fix a joint.

Related: why one cell reaches the cutoff first, and what the cell voltage delta actually tells you.

JK BMS Remote is an independent remote monitoring solution compatible with JK-BMS products. JK BMS Remote is not affiliated with, endorsed by, or sponsored by JK-BMS.

← All field notes